white film
I have had the white film. I assumed beerstone. I tried lots of acid. Turns out it was a silicate deposit from the biofine. As Dana states, the only solution was really hot caustic ( Birko Circ-u-late), 180ish for about an hour.
Cheers,
Rich DeLano
rich@thebrewinglair.com
I have had the white film. I assumed beerstone. I tried lots of acid. Turns out it was a silicate deposit from the biofine. As Dana states, the only solution was really hot caustic ( Birko Circ-u-late), 180ish for about an hour.
Cheers,
Rich DeLano
rich@thebrewinglair.com